  • jseklund
    Established Member
    • Aug 2006
    • 428

    #1

    Floor Finish

    Hopefully, this will be the last home-improvement question I have for a while. I have been fixing up a house now for 3 months, and many of you have already helped me greatly in different areas with your advice. I thank you all for the help (past, present and future!).

    As the project draws to a close, I am coming closer to the time where I will have to sand and refinishe the hardwood flooring. I have about 650 SF of white oak flooring that was in the house when I bought it, and in serious need of refinishing. I also knocked down a wall to create a formal dining room. In this room I have put down a Maple transition piece in the 2 doorways (against some other people's advice- but I think it'll come out nicely) and then put new cherry flooring down in the dining room. So, I have a room with a doorway on 2 walls and a cherry floor. In the doorway is Maple, on the other side of the maple in both doors is the oak flooring in the hall and living room.

    I am going to rent a sander, and had the opportunity to use one of them at a friend's house about a month ago- I feel confident there. I am thinking of using the edge sander or ROS on the transition piece to keep the bleeding of different woods to a minimum.

    The question is on the finish. I am going with a high-solids "gym floor" finish for the final 2 coats. However, in playing around a little with some scraps, I put 2 coats of Teak Oil on the different pieces of wood and then finished with regular poly. I liked the way the Teak Oil popped out the grain patterns.

    I already know I'm going to have to be careful not to over-sand the cherry or I'll get a blotchy look in the wood from the Teak Oil. Is there anything else I should be aware of? Is there any reason I should avoid the teak oil and just use the floor finish by itself?

    Thanks in advance for the help!
    F#$@ no good piece of S#$% piece of #$@#% #@$#% #$@#$ wood! Dang. - Me woodworking
  • Hellrazor
    Veteran Member
    • Dec 2003
    • 2091
    • Abyss, PA
    • Ridgid R4512

    #2
    Which gym floor finish are you using? I use the high solid oil based finish at work. My only concern is the "for the final 2 coats" clause. Even on a new floor, I've only used 2 coats max and that was the older higher VOC products. In fact the newer low VOC, high solid finish only requires 1 coat.


    http://www.valsparflooring.com/valsp...s/TDS-WP14.pdf

    Comment

    • jseklund
      Established Member
      • Aug 2006
      • 428

      #3
      Hellrazor,
      I remember you mentioning the Valspar. I didn't find anything quite like that, but my gf owns a cleaning company and uses a lot of Amrep Misty products. They make a 40% solids, oil modified finish that I will be using. They generally make extraordinary stuff, so I'm hoping the finish will be no exception. However, most retail users would never know what Misty or Amrep are.....

      Anyway, I meant final two coats as in-

      1. Two coats of teak oil per label instructions
      2. Two coats of floor finish per label instructions.

      Basically I'm using the teak oil to bring out the wood characteristics, and then finishing as if it were anything else.

      The Valspar stuff looks great....I couldn't find anywhere to get it though
      F#$@ no good piece of S#$% piece of #$@#% #@$#% #$@#$ wood! Dang. - Me woodworking

      Comment

      • Hellrazor
        Veteran Member
        • Dec 2003
        • 2091
        • Abyss, PA
        • Ridgid R4512

        #4
        You might have trouble getting valspar because of the VOC regs. They have been trying to get me to switch to water based finish and I have been kicking and screaming the whole way. I have a presentation with a picture of our gym floor, I need to see if I can extract it.

        Just make sure you are able to bond the 2 finish layers without the need to scuff the first coat. 2 coat finish is made to chemically bond the 2nd coat to the 1st within 24 hours. If you go over 24hours you need to scuff/sand or disc the floor again. I am not sure if a 1 coat system will chemically bond or not when applying a second coat.